Resysta - The future material

The material Resysta Already today, Resysta meets tomorrow´s technical and ecological demands. Owing to the high durability and sustainability Resysta offers, completely new applications are possible. The fibre reinforced hybrid material is produced of approx. 60% rice husks, approx. 22% common salt and approx. 18% mineral oil, which makes it both environmentally friendly as well as extremely weather resistant against sun, rain, snow or salt water. At the same time, Resysta requires minimal care and offers the look and feel of wood. Water resistant surfaces with the look of wood are Resysta´s future. Wait and see!

One material, endless possibilities
WaWater resistant, sustainable and almost identical to tropical wood – all these characteristics open a variety of possibilities in using Resysta. Outdoor furniture, floor coverings and decks of ships are just the beginning. Further examples are house facades, wellness and wet areas. Resysta is not subject to any fluctuations in size caused by humidity and therefore is perfectly suitable for surface treatment. Whatever the future will look like – it is made of Resysta.

Minumum care maximum look
Resysta is sophisticated as far as its look is concerned, but not very demanding in maintenance. The fibre reinforce hybrid material is absolutely water resistant. Therefore, cracks and splinters are a thing of the past. Also insects and fungi cannot harm Resysta. In terms of maintaining Resysta, the most important thing is:lean back and enjoy!

A good feeling with Resysta

Resysta does not only look like wood – it also feels like it. In order to achieve the typical “tropical wood feeling” a special procedure is applied. To touch Resysta does not only feel good, it also surpasses nature´s model in this respect. Thanks to its special composition, the surface stays free from cracks and splinters in the long term. Injuries caused by wooden splinters are therefore a thing of the past. Even after years, the future material ensures an agreeable feeling.

Resysta Materialeigenschaften


Anyone working with wood will be enthused about Resysta. Like its natural model it can be sawn, drilled, painted, sanded or oiled. However, there is one decisive advantage: Resysta does neither crack nor splinter and its cutting wastes are 100% recyclable. The different profiles of Resysta are produced in an extruderand can be used for many applications.

Material Resysta
Homogenous extrusion
Raw materials used
Raw materials used Rice husks
Common salt
Mineral oil
approx. 60%
approx. 22%
approx. 18%
Material Characteristics
Density  ASTM D2395:2002 approx. 1.46 g/cm³
Coeffivient of linear
thermal expansion
 ASTM D696 3,6 x 10(-5) mC
Water Absorption & Humidity ASTM D1037:2006a Little up to no water absorption (only surface moistening)
Weathering and
UV Resistance
QUV Test With glaze treatment, Resysta surfaces are extremely resistant
Slippery Test (wet area barefoot) DIN 51097 Class C (highest class)
Fire Rating (german/european norm) EN ISO 11925-2 B2 (E) - standard flammable (with additional treatment B1 reachable)
Fire rating according NFPA (US Norm) ASTM E84 Class A (flame propagation 25, smoke emission 450)
Fire rating (British standard) BS 476 Teil 6&7  Class 1
Duraility Resistance against wood-destroying fungi (basidiomycetes) DIN V EN V 12038:2002 the material has not been affected,
highest durability
- Class 1
Emission LGA-tested safety & contamination LGA test passed
Brinell hardness (HB) EN 1534 81,1 N/mm2
Coefficient of sliding and friction μ untreated EN 13893 0,46
Coefficient of sliding and friction μ with 2K varnish EN 13894 0,52
Axial Witdrawal Force (of Screws) EN 320.2011-07 5777 N
Thermal Conductivity (λ) EN 12664 0.199 W/(mK)
Water Vapour Transmission DIN EN ISO 12572 5777 N
Bending Strength ISO 178 46 N/mm²
Bending Modulus ISO 178 3850 N/mm²
Tensile Strength ISO 527 21,8 N/mm²
Tensile Modulus ISO 527 2340 N/mm²
Tensile Modulus ISO 527 2340 N/mm²
Shearing Strength EN 392 16,8 N/mm²
Durability - Resistance against rotting fungi CEN/TS 15083-2 No attack by the test fungi, highest durability class 1 (very durable)
Durability against mold fungi and wood discoloring fungi EN 15534-1:2012 Durability against the wood discoloring fungi (very durable)
Durability against subterranean Termites ASTM D3345-08 High Durability against subterranean Termites - nearly no weight loss
Specific surface and volume resistances DIN IEC 60093 measuring voltage 100 V Surface resistance Rx=8,0*10(13) Ω
Specific surface resistance α=8,1*10(14) Ω
Volume resistance Rx=2,2*10(13) Ω
Specific volume resistance α=6,3*10(14) Ω
Work Like wood with wood processing machines: Cutting, milling, drilling, sanding, gluing and screwing
Surface treatment Applying original Resysta stain and 2K sealer with brush


Properties Resysta Tropical wood Indegenious Lumber WPC
Haptics ++ ++ + -
Water resistance ++ - - -
UV resistance ++ -- -- -
No fungal decay ++ + +/- +
No graying and fading ++ + +/- +
Processing + + + +
Life time ++ - - +
Recyclability ++ +/- - -
Paintability + + + -
No cracking ++ - - +
No splintering ++ - - +
No swelling ++ - - -
Glueability + +/- + -
Fire resistance + + + -



Opening hours „Resysta Partner Summerfield“
Tue – Fri: 10.00 – 18.00 Uhr
Sat : 10.00 – 16.00 Uhr

Business hours Office Resysta
Mon – Thu: 08.30 – 17.00 Uhr
Fri : 08.30 – 14.00 Uhr
or upon agreement on the phone

Hochstraße 21
82024 Taufkirchen bei München